Muhammad Sulistiyo Aji's scientific contributions

What is this page?


This page lists the scientific contributions of an author, who either does not have a ResearchGate profile, or has not yet added these contributions to their profile.

It was automatically created by ResearchGate to create a record of this author's body of work. We create such pages to advance our goal of creating and maintaining the most comprehensive scientific repository possible. In doing so, we process publicly available (personal) data relating to the author as a member of the scientific community.

If you're a ResearchGate member, you can follow this page to keep up with this author's work.

If you are this author, and you don't want us to display this page anymore, please let us know.

Publications (1)


Fig. 4. A) Joint of 2 clamps at 3 mm thick, B) Joint of 4 clamps thick 3 mm, C) Joints 2 clamps plate thickness 5 mm, D) Joints 4 clams plate thickness 5 mm, E) Joint 2 clamps on a plate thickness of 9 mm, F) Joint 4 clamps on a plate thickness of 9 mm.
Fig. 5. Temperature distribution for plate thickness of 3 mm, 5 mm, and 9 mm
Fig. 6. Microstructure of joint clamps with thickness of 3 mm (A-C), 5 mm (D-F), and 9 mm (G-I)
Fig. 7. Vickers microhardness test of plate
Fig. 8. Maximum shear force of clamp joints
Lap Joint on St.37 Steel Plate with Friction Welding Clamping Method
  • Article
  • Full-text available

June 2023

·

29 Reads

Journal of Mechanical Engineering Science and Technology (JMEST)

·

Nugroho Santoso

·

Wiyadi Wiyadi

·

[...]

·

Achsan Tarmudi

Friction stir (FW) welding is a relatively fresh method that was created and has been continually refined and adapted to industrial applications due to its benefits. This approach for solid-state joining entails connecting the components at a temperature below their melting point and then heating them up. Clamp joint applications are widely used using external heating and hitting with high strength, but the clamped joints with the FW method are rarely done. The research studied the characteristic of clamped joints at various plate thicknesses using the FW method. In this study, 30 specimens were used in the form of a St.37 low carbon steel plate with a size of 50 mm x 100 mm and a thickness of 3 mm, 5 mm, and 9 mm, and several holes were made with a diameter of 5 mm. The plate was connected by 2 clamps, and 4 clamps then the FW method was conducted in a milling machine. The results indicate that the plates were connected well. The highest hardness value was 256.4 VHN on the FW of 9 mm plate. The microstructure is dominated by ferrite and a little pearlite phase. The largest shear force is 66.54 kN obtained at 4 clamps with a plate thickness of 9 mm, and the lowest is 13.46 kN, obtained at 2 clamps with a plate thickness of 3 mm.