Question
Asked 15th Apr, 2020
What is the relationship between bulking factor vs SG vs Material compaction?
What is the relationship between bulking factor vs SG vs Material compaction? What tests can be done to calculate and assign or review material SG? (i.e stockpile material or compacted rill material)
Similar questions and discussions
Related Publications
Several methods are available for determining the bulk specific gravity (G(sb)) of reclaimed asphalt pavement (RAP). However, a clear recommendation has not been had for determining this property. In this study, asphalt mixes with known aggregate properties were produced and aged in the laboratory to simulate RAP. The aggregates were recovered, and...