The Co3O4 films were prepared by using two steps method. Initially, the films
were deposited on thoroughly cleaned copper substrates by using pulsed DC
electrochemical deposition method from a solution containing Co(NO3)2:6H2O
and H3BO3. The films were deposited at different molar concentrations: 0.1, 0.2,
0.3, 0.4, 0.5, 0.6 and 0.7 M of C...
Similar publications
We report on the challenges in a hybrid sub-micrometer fabrication process while using three dimensional femtosecond direct laser writing and electroplating. With this hybrid subtractive and additive fabrication process, it is possible to generate metallic polarization elements with sub-wavelength dimensions of less than 400 nm in the cladding area...