Fig 8 - available via license: Creative Commons Attribution-NonCommercial-NoDerivs 3.0 Unported
Content may be subject to copyright.
Comparing temperature behavior of strain gauge sensors on polyimide and thin glass substrates
Source publication
In this paper we present a flexible sensor element with low power consumption and long-term stability under typical aeronautical conditions. Titanium (Ti) is used as thin film metallization material, because of its high corrosion and heat resistance. Polyimide foil and also ultrathin glass substrates are used as substrate. Parylene C is used as pas...
Context in source publication
Context 1
... strain gauge sensors on polyimide and thin glass substrate are investigated in the temperature range from -30 °C to + 80 °C in increasing and decreasing steps. The temperature behavior of strain gauge sensors on polyimide and thin glass substrates are show in figure 8. Sensors on polyimide substrate showing higher temperature hysteresis in compare to the sensors on thin glass substrate. ...